Surface analysis on organic light emitting diodes
The main theme of this work is the application of various surface analysis techniques, including ultraviolet photoelectron spectroscopy (UPS), X-ray photoelectron spectroscopy (XPS), Auger electron spectroscopy (AES) and atomic force microscopy (AFM), to the study of several issues related to the operating